Nanoscale Coatings Improve Stability and Efficiency of Devices for Renewable Fuel Generation

Splitting water into its components, two parts hydrogen and one part oxygen, is an important first step in achieving carbon-neutral fuels to power our transportation infrastructure – including automobiles and planes.

Now, North Carolina State University researchers and colleagues from the University of North Carolina at Chapel Hill have shown that a specialized coating technique can make certain water-splitting devices more stable and more efficient. Their results are published online in two separate papers in the Proceedings of the National Academy of Sciences. (more…)