Nanoscale Coatings Improve Stability and Efficiency of Devices for Renewable Fuel Generation

Splitting water into its components, two parts hydrogen and one part oxygen, is an important first step in achieving carbon-neutral fuels to power our transportation infrastructure – including automobiles and planes. Now, North Carolina State University researchers and colleagues from … Continue reading